Started grinding crazing crazy cracks and found semi sub standard old repair,, to grind completely out( air in previous glass) , or epoxy fair ,add glassover, or just fair it out and prime… the boat is a complete refit rerig.
Looking for thoughts ,fairing seems the quikest
 

Attachments

  • IMG_1165.jpeg
    IMG_1165.jpeg
    111.1 KB · Views: 24
  • IMG_1018.jpeg
    IMG_1018.jpeg
    119.5 KB · Views: 24

bgary

Advanced Beginner
Blogs Author
If it is just gelcoat crazing, and you're planning to paint, I'd just fair and paint.

If on the other hand they are "cracks" - meaning, they pass through gelcoat to the laminate, then yeah, grinding and filling is probably the right long-term fix.
 